Detail Information
Elongation: 150% Flame Rating: 94 V-0
Specific Gravity: 1.8g/cm3 Tensile Strength: 150 Psi
Application: LED Industrial/cell Phone Industrial/computer Pc Industry, Etc Type: Insulation Sheet
Applicate Temperature(℃): -45 To 120 Material: Polyimide
High Light:

150psi silicone free thermal pad

,

1.8g/cm3 thermally conductive gap filler

,

150psi thermally conductive gap filler


Product Description

High Performance Tensile Strength 150psi Silicone-Free Thermal Pad For CUP/GPU
 
Product Description
 

  Non-silicone thermal pads are base on special resins. They donot make circuit failure ,because they donot have siloxane volatilization and silicone oil seeping. The products have good tensile strength and wear resistance, it can solve the problem of traditional silicone thermal pad such as gases vapors and silicone oil separation when it use . This product is capable of electrolytic liquid which made this material in the lithium battery industry has great development prospect.

 
Phisical Properties
 
 
Product Name
Non-silicone thermal pad
*
 
Color
White
Visual
 
Thickness
0.25 ~ 5.0mm
ASTM D374
 
Specific Gravity
1.8g/cm3
ASTM D792
 
Thermal Conductivity
1.50 W/mK
ASTM D5470
 
Hardness(shore oo)
50~90.
ASTM D2240
 
Elongation
150%
ASTM D412
 
Tensile Strength
150psi
ASTM D412
 
Electrical strength
>200VAC/mil
ASTM D149
 
Flammability Rating
94 V-0
UL 94
 
Volume Resistivity
1013Ω.cm
ASTM D257
 
Operating Temperature
-40 ~ 120℃
——
 
Thermal Resistance(1mm,@40psi)
1.0℃*in2/W
ASTM D5470
 
Compression Ratio(1mm,@40psi)
30%
——
 
RoHS (10)
PASS
IEC 62321
 
Halogen (4)
PASS
EN14582
 
REACH(191)
PASS
EN14372

 

 

Product Details

 

1.8g/Cm3 150psi Silicone Free Thermal Pad For GPU 01.8g/Cm3 150psi Silicone Free Thermal Pad For GPU 1

 

 

 

 

 
1.8g/Cm3 150psi Silicone Free Thermal Pad For GPU 2
FAQ
 
Q1: What thermal conductivity test method was used to achieve the values given on the data sheets?
A1: A test fixture is utilized that meets the specifications outlined
in DRL-III.

Q2: Is GAP PAD offered with an adhesive?
A2: Currently, All GAP PAD Materials have inherent tack.

Q3: Is the adhesive reuse?
A3: Depending on the surface being applied to, if care is taken, the pad may be reuse. Special care should be taken.When removing
the pad from aluminum or anodized surfaces to avoid tearing or delamination.

Q4: What is meant by “natural tack”?
A4: The characteristic of the rubber itself has a natural inherent tack, with the addition of an adhesive. As with adhesive backed
products, the surfaces with natural tack may help in the assembly process to temporarily hold the pad in place while the
application is being assembled. Unlike adhesive backed products, inherent tack does not have a thermal penalty since the rubber
itself has the tack. Tack strength varies from one GAP PAD product to the next.

Q5: Can GAP PAD with natural tack be repositioned?
A5: Depending on the material that the pad is applied to, in most cases they are repositionable. Care should be taken when
removing the pad from aluminum or anodized surfaces to avoid tearing or delaminating the pad. The side with the natural tack is
always easier to reposition than an adhesive side.

Q6: Is GAP PAD reworkable?
A6: Depending on the application and the pad being used, GAP PAD has been reworked in the past. Some of our customers are
currently using the same pad for reassembling their applications after burn-in processes and after fieldwork repairs. However,this
is left up to the design engineer’s judgment as to whether or not the GAP PAD will withstand reuse.

Q7: Will heat make the material softer?
A7: From -40°C to 200°C, there is no significant variance in hardness for silicone GAP PAD Materials and Gap Fillers.

Q8: What is the shelf life of GAP PAD?
A8: Shelf life for most GAP PAD Materials is ten (10) year after the date of manufacture. For GAP PAD with adhesive, the shelf
life is two (2) years from the date of manufacture. After these dates, inherent tack and adhesive properties should be
recharacterized. The GAP PAD material’s long-term stability is not the limiter on the shelf life; it is related to the adhesion or
“age up” of the GAP PAD to the liner. Or in the case of a GAP PAD with adhesive, the shelf life is determined by how the adhesive
ages up to the removable liner.
Q9: How is extraction testing performed?
A9: The test method used is the Soxhlet Extraction Method;

Q10: What is the thickness tolerance of your pads?
A10: The thickness tolerance is ±0.2mm on materials .

Q11: What are the upper processing temperature limits for GAP PAD and for how long can GAP PAD be exposed to them?
A11: GAP PAD in general can be exposed to temporary processing temperatures of 120°C.Time base on GAP PAD thickness, assembly line
14 meters long,time about 10-15 minutes .

Q12: Is GAP PAD electrically isolating?
A12: Yes, all GAP PAD materials are electrically isolating. However, keep in mind that GAP PAD is designed to fill gaps and it is
not recommended for applications where high mounting pressure is exerted on the GAP PAD.

Q13: Why are “wet out,” “compliance” or “conformability” characteristics of GAP PAD important?
A13: The better a GAP PAD lays smooth “wets out” or conforms to a rough or stepped surface, giving less interfacial resistance
caused by air voids and air gaps. GAP PAD Materials are conformable or compliant as they adhere very well to the surface. The GAP
PAD Materials can act similarly to a “suction cup” on the surface.
This leads to a lower overall thermal resistance of the pad between the two interfaces.

Q14: Is anything given off by the material (e.g., extractables, outgassing)?
A14: Silicone GAP PAD and Gap Fillers, like all soft silicone materials, can extract low molecular weight silicone .Also note that
GAP PAD and Gap Filler have some of the lowest extraction values for silicone-based gap filling products on the market and if
yourapplication requires minimal silicone, see our line of silicone-free material. The White Paper on GAP PAD S-Class and
information about our silicone-free materials are available on our website.

Q15: Why does the Technical Data Sheet describe the Shore hardness rating as a bulk rubber hardness?
A15: A reinforcement carrier is generally used in BERGQUIST GAP PAD Materials for ease of handling. When testing hardness, the
reinforcement carrier can alter the test results and incorrectly depict thinner materials as being harder. To eliminate this
error, a 250 mil rubber puck is molded with no reinforcement carrier. The puck is then tested for hardness. The Shore hardness is
recorded after a 30-second delay.